DENDRITE EXP
Base Synthetic Rubber
Application   Leather, engineering, flooring, automobile, electronics & similar  others.
Solvent Aromatic and Aliphatic Solvent Combination
Solid Content Approximately 20%
Colour   Tan
Viscosity 1850  - 2100 cps at 30 degree Centigrade
Method of Application Make sure that the surfaces to be bonded are even, clean, dry and free from grease/oil. A coat of adhesive is to be applied uniformly on both the surfaces to be joined. Porous substrate like leather may require two coats for superior bonding. Wait for 10 minutes to allow the solvent to evaporate. Place the coated surfaces one above other, while the adhesive remains tacky. Press the coated surfaces firmly together.  
Caution Highly inflammable. Replace lid immediately after partial use. Store in a cool and dry place.
Packing 20 ltrs, 5 Ltrs, 1ltr